Skip to content

Brief introduction of crevice corrosion test project

Crevice corrosion is the phenomenon that metal surfaces form gaps due to the presence of foreign objects or structural reasons, resulting in accelerated metal corrosion in the gaps.

Test device

The width of the slit or gap that causes crevice corrosion must be sufficient to allow the medium to enter and stay in it. When the crevice width is between 25 and 100 μm, it is the most sensitive range for crevice corrosion. In some wider crevices, the corrosive medium is easy flowing, crevice corrosion generally does not occur.

The result of crevice corrosion will lead to a reduction in the strength of the component and a poor fit. The increase in the volume of corrosion products in the crevices will cause local additional stress, which not only makes assembly difficult, but may also reduce the bearing capacity of the component.

Crevice corrosion of metals shows the following main features:

(1) Whether it is the contact of the same or different metals or the contact between the metal and the non-metal, or even some deposits and attachments on the metal surface, as long as there are slits and corrosive media that meet the crevice corrosion, almost all crevice corrosion occurs in both alloys and metals.

Alloys or metals with strong self-passivation ability are more sensitive to crevice corrosion.

(2) Almost all media (including fresh water) can cause crevice corrosion of metals, and the solution containing chloride ions is the most likely to cause crevice corrosion.

(3) The surface of the metal subjected to crevice corrosion can be either comprehensive corrosion or pitting corrosion. Materials with good corrosion resistance usually show pitting corrosion, while materials with poor corrosion resistance usually show full corrosion.

(4) The crevice corrosion has a gestation period, and its length is different due to different materials, crevice structure and environmental factors.( i.e.: The crevice corrosion speed of stainless steel pipes or stainless steel flanges in dry environment will be slower than that in wet environment) The crevices of crevice corrosion are often covered by corrosion products, thereby enhancing the occlusion effect of the crevices.

crevice corrosion in metal

Test methods and standards of crevice corrosion

ASTM G48 methodB Crevice corrosionGB/T 10127 Crevice corrosion
ASTM G48 methodD Critical crevice corrosion temperature of nickel-based chromium-containing alloy for bearingsGB/T 13452.4 Filament corrosion test on metal surface
ASTM G48 methodF Critical crevice corrosion temperature for stainless steelGB/T 26323 Filament corrosion test on aluminum and aluminum alloy surface
 JB/T 5326 Crevice corrosion test of metal materials for instrument

Crevice corrosion sample requirements
Crevice corrosion sample size requirements: length 50mm, width 25mm, thickness is the actual thickness, preferably 2 ~ 3mm. The surface of the sample must be flat.

Evaluation of seam removal corrosion test
1. Crevice corrosion: weightlessness corrosion rate,
2. Crevice corrosion electrochemistry: corrosion potential, polarization current vs. time curve, corrosion observation

Crevice corrosion sample pictures and test charts

en_USEN
logo of Kaysuns

Welcome to contact us

Supplying of Stainless & Alloy Piping Material

  • Need an offer ?
  • Want to know the dimension / catalog ?
  • Talk about the technical issues ?

Feel free to contact us, and we will be more than happy to answer all of your questions.

Get a Free Quote Now

small_c_popup.png

Get a free Quote now

Do you want to learn more? Contact us

We will reply you in 24 hours. Thank you!